Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00427 - 2.62 GPa | 0.620 - 380 ksi | Average value: 0.743 GPa Grade Count:7 |
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 0.00427 GPa | 0.620 ksi | ASTM D790 |