Mechanical Properties Metric English Comments
Flexural Modulus 0.659 GPa
95.6 ksi
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou..