Polymer Property : Flexural Modulus = 0.68200 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.68200 GPa
98.916 ksi
ASTM D790
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.