Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.689 GPa | 100 ksi | 1% Secant; ASTM D790 |
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized. Available as natural and several colors powder compounds.High quality Polyethylene re.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
Network Polymers NPP 11-0535 Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-1902 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | 1.3mm per min; ASTM D790 |
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | 1.3mm per min; ASTM D790 |
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | 2% Secant - Method 1; ASTM D790 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
Multibase Multi-Flamâ„¢ 0501 PP Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionBlow MoldingUses:TubingPipingInformation provided by Multibase |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 835 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | at 1% secant; ASTM D790 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | at 1% secant; ASTM D790 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | at 1% secant; ASTM D790 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | 0.05 in/min; ISO 178 |
CTC X-PRO CTC PP 4025 Polypropylene Copolymer X-PRO PP 4025 is a high value polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | 1% secant; ASTM D790 |
ExxonMobil LLP8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.689 - 0.690 GPa | 100 - 100 ksi | Average value: 0.690 GPa Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |