Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
PolyMirae Moplen EP200R Injection Molding Grade Polypropylene Moplen EP200R is the reactor TPO manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP200R is a super impact copolymer particularly suitable for injection molding of.. |
|||
Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
Hyosung Topilene C500H PP C500H Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
Hyosung Topilene C600H2 PP C600H2 Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.735 GPa | 107 ksi | Olsen Stiffness; ASTM D747 |
Global F-8000 High Density Polyethylene Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation. |
|||
Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
LG Chemical LUTENE-H ME5000 HDPE Description: LUTENE-H ME5000 is mainly intended for injection molding of containers and bottle cap. It has good stress cracking resistance and high impact strength.Applications: Containers, dust bin.. |
|||
Flexural Modulus | 0.735 GPa @Thickness 6.40 mm |
107 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL TE5007B PP+Rubber, High Impact Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical |