Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.772 GPa | 112 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-1010 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-2010 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | ASTM D790 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.772 - 1.17 GPa | 112 - 170 ksi | Average value: 0.903 GPa Grade Count:12 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | 2% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | |
Dow HDPE 42047N High Density Polyethylene DOW HDPE 42047N resin is a narrow molecular weight distribution copolymer designed to combine high impact strength and environmental stress crack resistance with excellent processability over a wide.. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | ASTM D790 |
Lucent Polymers TPO-10T Thermoplastic Polyolefin, 10% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 0.772 GPa | 112 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |