Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
SABIC M200056 High Density Polyethylene for Injection Molding Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |