Polymer Property : Flexural Modulus = 0.868 GPa
Polymer Property :
Flexural Modulus =
0.868 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
0.868
GPa
126
ksi
ISO 178
Breplast Bretene SP Polypropylene / Polyethylene Composite
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.