Polymer Property : Flexural Modulus = 1.04 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.04 GPa
151 ksi
Tangent, 1.3 mm/min; ASTM D790
Flint Hills 23S1Acs256 Random Copolymer Polypropylene
Features: High contact clarity, blush resistant, good impact and flexural modulus. Product does not contain animal derived components.Applications: Blow molded articles - Food, health, medical an..
Flexural Modulus 1.04 GPa
151 ksi
Tangent; ASTM D790
Flint Hills P5M6K-101X Random Copolymer Polypropylene
Features: Excellent clarity and processing. Product does not contain animal derived components. Phthalate-freeApplications: Injection molding - high clarity parts and medical devicesInformation ..
Flexural Modulus 1.04 GPa
151 ksi
2% secant; ASTM D790-02
Ipiranga Petrochem GF 4950 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Flexural Modulus 1.04 GPa
151 ksi
ASTM D790
Multibase Multi-Flamâ„¢ 2318 PP Polypropylene
Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingFurnitureInformation provided by Multibase
Flexural Modulus 1.04 GPa
151 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DMDA-8980 NT 7 High Density Polyethylene Resin
DOW DMDA-8980 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow
Flexural Modulus 1.04 GPa
151 ksi
ASTM Test
BASF Ultramid® 8281 HS PA6 (Dry)