Polymer Property : Flexural Modulus = 1.3053 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0089997 GPa
1.3053 ksi
ASTM D790
Sekisui PIOCELAN TOPF-40DB Flame Retardant Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..