Mechanical Properties Metric English Comments
Flexural Modulus 1.372 GPa
199.0 ksi
ASTM D790-95
Multibase Multi-Pro® 2510 XGW High Gloss Polypropylene
PP High Gloss compound formulated for small appliances such as food-processors and coffee machines. This product is high heat stabilized for use in irons and other appliances with elevated temperat..