Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Flexural Modulus | 0.882 - 1.372 GPa | 128 - 199.0 ksi | ASTM D790 |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |