Polymer Property : Flexural Modulus = 1.414 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.414 GPa
205.1 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 0110 X Natural Polypropylene
This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide..
Flexural Modulus 1.414 GPa
205.1 ksi
12.5 mm/min; ASTM D790
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade
ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case..