Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.518 GPa | 220.2 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |