Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.575 GPa | 228.4 ksi | ASTM D790 |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |
|||
Flexural Modulus | 1.575 GPa | 228.4 ksi | ASTM D790 |
Eastman Tritan MX730 Copolyester Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Flexural Modulus | 1.575 GPa | 228.4 ksi | ASTM D790 |
Eastman Tritan MX731 Copolyester Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Flexural Modulus | 1.575 GPa | 228.4 ksi | ASTM D790 |
Eastman Tritan TX1500HF Copolyester Eastman Tritan TX1500HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1500HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1000. Other outstanding features.. |
|||
Flexural Modulus | 1.575 GPa | 228.4 ksi | ASTM D790 |
Eastman Tritan TX1501HF Copolyester Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester.. |