Polymer Property : Flexural Modulus = 1.663 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.663 GPa
241.2 ksi
ISO 178
S&E Specialty Polymers TufFill™ 5003UV Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..
Flexural Modulus 1.663 GPa
241.2 ksi
ASTM D790
Kolon KOCETAL® UR304 Toughened Grade Acetal Resin
TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon.