Flexural Modulus 1.703 GPa
247.0 ksi
ISO 178
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry)
Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o..