Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.710 GPa | 248.1 ksi | ASTM D790 |
Lucent Polymers PC/PBT-1420IM Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |