Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0124 GPa | 1.80 ksi | 1% secant; ASTM D790 |
ExxonMobil Escorene® UL 7840E Adhesive Application Resin Escorene Ultra UL 7840E is a 31.4% vinyl acetate copolymer that has good compatibility with both hydrocarbon and natural tackifiers and is suitable for making hot melt adhesives adn sealants. UL 784.. |