Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.863 GPa | 270.2 ksi | ASTM D790 |
RedEye On Demand PC/ABS for FDM Rapid Prototyping This thermoplastic polymer blend combines PC (Polycarbonate) and ABS (Acrylonitrile Butadiene Styrene) to produce an industrial material with a lot to offer. It combines the strength of PC with the .. |
|||
Flexural Modulus | 1.863 GPa | 270.2 ksi | ASTM D790 |
Stratasys® PC-ABS PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior mechanical properties and heat resis.. |
|||
Flexural Modulus | 1.863 GPa @Temperature 260 °C |
270.2 ksi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the .. |