Polymer Property : Flexural Modulus = 1.961 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.961 GPa
284.4 ksi
ASTM D790
Kolon KOPA® KN333NW High Impact Nylon 66
Impact -resistant, dimensional safetyApplications Wheel coversInformation provided by API-Kolon.
Flexural Modulus 1.961 GPa
284.4 ksi
ASTM D790
Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin
High elastic, whether resistantApplications: WipersInformation provided by API-Kolon.