Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.965 GPa | 285.0 ksi | ASTM D790 |
Ineos Nova 6200 Super High Impact Polystyrene Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
Flexural Modulus | 1.965 GPa | 285.0 ksi | ASTM D790 |
Ineos Nova 6201 Super High Impact Polystyrene Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
Flexural Modulus | 1.965 GPa | 285.0 ksi | ASTM D790 |
Ineos Nova 6260 Super High Impact Polystyrene
(discontinued **) Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |