Polymer Property : Flexural Modulus = 10.66 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.66 GPa
1546 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DE004ER PC
LNP* STAT-KON* DE004ER is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added featuresof this material include: Electrically Conductive, Easy Molding, Mold Release.