Polymer Property : Flexural Modulus = 10.81 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.81 GPa
1568 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RV0079 PA 66
LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural.