Polymer Property : Flexural Modulus = 101.5 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.6998 GPa
101.5 ksi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0437C10L1 Calcium Reinforced
Flexural Modulus >= 0.6998 GPa
>= 101.5 ksi
ASTM D790
Buckeye Polymers BP FLEX D6020 BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Flexural Modulus >= 0.6998 GPa
>= 101.5 ksi
ASTM D790
Buckeye Polymers BP FLEX D6020 U BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Flexural Modulus 0.6998 - 1.03 GPa
101.5 - 150 ksi
ASTM D790
Buckeye Polymers BP FLEX D6020-08 BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..