Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.415 GPa | 1655.6 ksi | ASTM D790 |
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |