Flexural Modulus 11.43 GPa
1658 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF0069SF PA 66
LNP* THERMOCOMP* RF0069SF is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Flexural Modulus 11.43 GPa
1658 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF0069SF PA 66 (Asia Pacific)
LNP* Thermocomp* RF0069SF is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Flexural Modulus 11.43 GPa
1658 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM HU2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Flexural Modulus 11.43 GPa
1658 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Flexural Modulus 11.43 GPa
1658 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..