Polymer Property : Flexural Modulus = 11.81 GPa
Polymer Property :
Flexural Modulus =
11.81 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
11.81
GPa
1713
ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT
LNP THERMOCOMP* WF008 is a compound based on PBT resin containing 40% Glass Fiber.