Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.93001 - 113 GPa @Temperature 65.6 - 177 °C |
570.009 - 16400 ksi @Temperature 150 - 350 °F |
Average value: 32.8 GPa Grade Count:2 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Flexural Modulus | 1.10 - 113 GPa | 160 - 16300 ksi | Average value: 10.5 GPa Grade Count:272 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |