Flexural Modulus 0.0840 GPa
12.2 ksi
1.7 mm/min; DIN 53457
Advanced Elastomer Systems VistaFlex® 714-B Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Flexural Modulus 0.0840 GPa
12.2 ksi
1.7 mm/min; DIN 53457
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Flexural Modulus 0.0840 GPa
12.2 ksi
ASTM D790
Arkema Group Pebax® 4033 Polyether Block Amide (PEBA)