Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.32 GPa | 1787 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Flexural Modulus | 12.32 GPa | 1787 ksi | 2 mm/min; ISO 178 |