Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.6 GPa @Temperature 23.0 °C |
1830 ksi @Temperature 73.4 °F |
Conditioned; ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Modulus | 12.6 GPa @Temperature 23.0 °C |
1830 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Modulus | 12.6 GPa | 1830 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL33 is a compound based on Polyethereketone resin containg Carbon Fiber, PTFE. Added features include: Elecrtically Conductive , Internally Lubricated. |
|||
Flexural Modulus | 12.6 GPa @Temperature 23.0 °C |
1830 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Modulus | 12.6 GPa @Temperature 23.0 °C |
1830 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Modulus | 12.6 GPa | 1830 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Modulus | 12.6 GPa | 1830 ksi | ASTM D790 |
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 12.6 GPa | 1830 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon ZX05043 PPE+PS (Europe-Africa-Middle East) LNP* Stat-kon* ZX05043 is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE, Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 12.6 GPa | 1820 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® T101G45 PET, 45% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 12.6 GPa | 1830 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PX94085 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PX94085 is a compound based on PA6 resin, containing Glass Fiber. |
|||
Flexural Modulus | 12.6 GPa | 1820 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® T101G45 PET, 45% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 12.6 GPa | 1830 ksi | ASTM D790 |
Plenco 08235 Polyester BMC, Compression Molded PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable .. |
|||
Flexural Modulus | 12.6 GPa | 1830 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |