Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0920 GPa | 13.3 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-613 EVA Injection Molding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 8.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This r.. |
|||
Flexural Modulus | 0.0917 GPa | 13.3 ksi | ASTM D790 |
Ecomass® 5100TU96 Tungsten Filled SEBS Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled SEBS Base ResinVery FlexibleInformation provided by Technical.. |