Polymer Property : Flexural Modulus = 136 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.940 GPa
136 ksi
ASTM D790
Flint Hills PP 23R2A Random Copolymer Polypropylene
Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: High contact clarity, non-blushing, toughness, impact, chemical..
Flexural Modulus 0.940 GPa
136 ksi
Kraton® G1650 + PP blend (20/80)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..
Flexural Modulus 0.940 GPa
136 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Solvay Engineered Polymers DEXFLEX® 930 TPO  (discontinued **)
Description: DEXFLEX® 930 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact propert..