Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.58 - 9.38 GPa | 1100 - 1360 ksi | Average value: 8.04 GPa Grade Count:7 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |