Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.9542 GPa | 138.4 ksi | 1% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |