Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.58 GPa | 1390 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications... |
|||
Flexural Modulus | 9.60 GPa @Temperature 23.0 °C |
1390 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® RE5231 BK533 PET
(Unverified Data**) Rynite® RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 9.585 GPa | 1390 ksi | ASTM Value |
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron 5233G is a 33% glass fiber reinforced, polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineerin.. |
|||
Flexural Modulus | 9.58 GPa | 1390 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF008 Acetal Copolymer (Europe-Africa-Middle East) LNP* THERMOCOMP* KF008 is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Flexural Modulus | 9.61 GPa | 1390 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 9.58 GPa | 1390 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific) LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized . |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABI.. |
|||
Flexural Modulus | 9.55 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Flexural Modulus | 9.58 GPa | 1390 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ASTM D790 |
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ASTM D790 |
Plenco 4466 Phenolic, Granular, Transfer Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ASTM D790 |
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET 40% GF/MF Reinforced, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Flexural Modulus | 9.55 GPa @Temperature 120 °C |
1390 ksi @Temperature 248 °F |
ASTM D790 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Flexural Modulus | 9.61 GPa | 1390 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 9.60 GPa @Temperature 23.0 °C |
1390 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Flexural Modulus | 9.57 GPa | 1390 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated. |