Flexural Modulus 14.2 GPa

@Temperature 23.0 °C
2060 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB SCANAMID 66 A12^ F50 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Modulus 14.2 GPa
2060 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6
LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive.
Flexural Modulus 14.2 GPa
2060 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 compound
Flexural Modulus 14.2 GPa
2060 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP 9X98026 PA 46 (Europe-Africa-Middle East)
LNP* Lubricomp* 9X98026 is a compound based on PA4.6 resin containing Barium Sulfate, PTFE and Carbon Fiber
Flexural Modulus 14.2 GPa
2060 ksi
ASTM D790
Covestro Petlon® DP3-1027 Semi-Crystalline PET, 45% Glass Fiber  (discontinued **)
Characteristics: General Purpose: Good Strength, High Rigidity and Heat ResistanceApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 4..
Flexural Modulus 14.2 GPa
2060 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66
LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Modulus 14.2 GPa
2060 ksi
ASTM D790
LNP Thermocomp® OF-1008 Polyphenylene Sulfide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..