Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.22 GPa | 2062 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear LNP* THERMOCOMP* OF008 is a compound based on PPS - Linear resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 14.22 GPa | 2062 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP OF008H PPS - Linear LNP* THERMOCOMP* OF008H is a compound based on PPS - Linear containing 40% Glass Fiber. Characteristics of this grade are: Healthcare. |