Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 14.7 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 14.7 GPa
2130 ksi
ISO 178
Nilit FRIANYL A63 GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 14.7 GPa
2130 ksi
ISO 178
Nilit FRIANYL A63 H-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 14.7 GPa
2130 ksi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Fibre Glast Epolite 2427 Epoxy  (discontinued **)
Information provided by Fibre Glast Developments Corporation.
Flexural Modulus 14.7 GPa
2130 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK
LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 14.7 GPa
2130 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK
LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant.
Flexural Modulus 14.7 GPa
2130 ksi
ISO 178
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Flexural Modulus 14.7 GPa
2130 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced
PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries.
Flexural Modulus 14.7 GPa
2130 ksi
ASTM D790
Sumitomo Bakelite North America SI 9041A Silicone Compound
SI 9041A is a long fiberglass reinforced silicone molding compound, which exhibits excellent high temperature properties in addition to good molding characteristics for transfer and compression mold..
Flexural Modulus 14.7 GPa
2130 ksi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced
PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries.
Flexural Modulus 14.7 GPa
2130 ksi
ISO 178
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned
Information provided by Unitika Ltd.
Flexural Modulus 14.7 GPa
2130 ksi
ASMT D790
Toyobo TS501 PPS, 50% Glass Fiber Reinforced
Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e..
Flexural Modulus 14.7 GPa
2130 ksi
ASTM D790
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Modulus 14.7 GPa
2130 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Copyright © lookpolymers.com All Rights Reserved