Mechanical Properties Metric English Comments
Flexural Modulus 14.715 GPa
2134.2 ksi
ASTM D790
E-Polymers SEPAZ® LA50 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Flexural Modulus 14.715 GPa
2134.2 ksi
ASTM D790
E-Polymers SEPAZ® LB60 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..