Mechanical Properties Metric English Comments
Flexural Modulus 15.32 GPa
2222 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear ..
Flexural Modulus 15.32 GPa
2222 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding.