Mechanical Properties Metric English Comments
Flexural Modulus 15.6 GPa
2260 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
Flexural Modulus 15.6 GPa
2260 ksi
ASTM D790
LNP Konduit® OTF-212-11 Polyphenylene Sulfide, Proprietary Filler  (discontinued **)
Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar..
Flexural Modulus 15.6 GPa
2260 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized.
Flexural Modulus 15.6 GPa
2260 ksi
ASTM D790
LNP Konduit® OTF-212-11 BK8-115 Polyphenylene Sulfide, Proprietary Filler  (discontinued **)
Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar..