Flexural Modulus 10.43 GPa
1513 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA
LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive..