Polymer Property : Flexural Modulus = 1535 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.58 GPa
1535 ksi
ASTM D790
Plenco 51130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform..
Flexural Modulus 10.58 GPa
1535 ksi
ASTM D790
Plenco 50240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..