Flexural Modulus 3.13711 - 109.075 GPa

@Temperature 50.0 - 177 °C
455.007 - 15820.2 ksi

@Temperature 122 - 350 °F
Average value: 63.0 GPa Grade Count:7
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..