Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0123 - 0.110 GPa | 1.78 - 16.0 ksi | Average value: 0.0398 GPa Grade Count:7 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |