Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.05 GPa | 1603 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 11.05 GPa | 1603 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |