Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.16 GPa | 168 ksi | 2% Secant-Method; ASTM D790 |
Ineos CP53-30 Polyethylene Copolymer CP53-30 is a high density polyethylene copolymer developed for corrugated piping applications. This product is recommended for use in applications that are required to meet AASHTO specifications M 2.. |
|||
Flexural Modulus | 1.16 GPa | 168 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 1.16 GPa | 168 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 1.16 GPa | 168 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Modulus | 1.16 GPa | 168 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 1.16 GPa | 168 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 63000CT PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Flexural Modulus | 1.16 GPa | 168 ksi | 1% secant, 0.5 in/min; ASTM D790B |
ExxonMobil PP7035E4 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Flexural Modulus | 1.16 GPa | 168 ksi | ASTM-D-790 |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |