Mechanical Properties Metric English Comments
Flexural Modulus 11.6 GPa

@Temperature 23.0 °C
1680 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Flexural Modulus 11.6 GPa
1680 ksi
5 mm/min; ISO 178
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Flexural Modulus 11.6 GPa
1680 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear
LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
Flexural Modulus 11.6 GPa
1680 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear
LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant.
Flexural Modulus 11.6 GPa
1680 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Flexural Modulus 11.6 GPa

@Temperature 23.0 °C
1680 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Flexural Modulus 11.6 GPa
1680 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific)
LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..
Flexural Modulus 11.6 GPa
1680 ksi
ASTM D790
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: ..
Flexural Modulus 11.58 GPa
1680 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp RF0069RS PA 66
LNP THERMOCOMP* RF0069RS is a compound based on Nylon 66 resin containing Glass Fiber, Mold Release, Flame Retardant. Added features of this material include: Easy Release.This data was supplied by..
Flexural Modulus 11.6 GPa

@Temperature 23.0 °C
1680 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Flexural Modulus 11.6 GPa
1680 ksi
ASTM D790
Plenco 08133 Polyester BMC, Compression Molded
PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Flexural Modulus 11.6 GPa
1680 ksi
ISO 178
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized
Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Flexural Modulus 11.6 GPa
1680 ksi
ISO 178-93
Wellman Wellamid® GF1662-GY1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
Flexural Modulus 11.6 GPa
1680 ksi
ISO 178
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Flexural Modulus 11.6 GPa
1680 ksi
ASTM D790
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant
Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo.